I don't know what I'm doing wrong... . but whatever it is I hope to correct it.
I have tried pre-heating, stainless steel wire brushing the ever living heck out of it, etc.
I'm using my machine on AC output, pure tunsten (balled) in the torch, and a boatload of amperage.
I can't get it to form a nice weld pool like regular old steel... . and when I do get a weld pool to form I'm usually at the point of turning my workpiece into a puddle of molten metal.
Any suggestions or tips?
Matt
I have tried pre-heating, stainless steel wire brushing the ever living heck out of it, etc.
I'm using my machine on AC output, pure tunsten (balled) in the torch, and a boatload of amperage.
I can't get it to form a nice weld pool like regular old steel... . and when I do get a weld pool to form I'm usually at the point of turning my workpiece into a puddle of molten metal.
Any suggestions or tips?
Matt