Everyone should get at least one sample analyzed.
Everything was good except, Molybdenum (47), Calcium (2808), Phosphorus (1162). These all seem to be anti-wear additives.
Lead was 5 with the average being 3, is this normal?
Fuel content was <0. 5, Antifreeze & Water were 0. 0
Iron was 16 with 55 being average, I wonder if my SuperPlug helped here
Silicon was 5PPM with the average being 12 so I assume my greased lip K&N in the factory box is doing it's thing.
PS, I love the spell checker thingy.
Everything was good except, Molybdenum (47), Calcium (2808), Phosphorus (1162). These all seem to be anti-wear additives.
Lead was 5 with the average being 3, is this normal?
Fuel content was <0. 5, Antifreeze & Water were 0. 0
Iron was 16 with 55 being average, I wonder if my SuperPlug helped here

Silicon was 5PPM with the average being 12 so I assume my greased lip K&N in the factory box is doing it's thing.
PS, I love the spell checker thingy.